TITLE:
An Integrated Statistical Framework for Evaluating Mechanical Durability and Lifecycle Performance of Photovoltaic Backsheets
AUTHORS:
Joseph Moses, Tridip K. Bardhan
KEYWORDS:
Photovoltaic Backsheet, Tensile Strength Degradation, Second-Order Polynomial Regression, Weighted Least Squares, Newey-West HAC, Serial Autocorrelation, Weibull Reliability, UV Exposure
JOURNAL NAME:
Journal of Materials Science and Chemical Engineering,
Vol.14 No.11,
November
27,
2026
ABSTRACT: Photovoltaic (PV) backsheets are subjected to continuous environmental stressors, resulting in gradual tensile strength degradation and reduced long-term module reliability. This paper presents a six-stage statistical modeling framework to quantify how cumulative ultraviolet (UV) exposure, temperature, relative humidity, and wind speed each contribute to tensile strength loss in a multilayer PPE-based PV backsheet (polyethylene terephthalate/polyethylene terephthalate/ethylene vinyl acetate, PET/PET/EVA). Pearson correlation using a field dataset of 511 sequential observations of cumulative UV doses (0.84 MJ/m2 to 271.6 MJ/m2) established UV irradiance as the most important degradation driver (r = −0.960, R2 = 0.921). Since the observations constitute one degradation time series, the serial autocorrelation was checked with the Durbin-Watson statistic and confirmed, necessitating Newey-West heteroscedasticity and autocorrelation-consistent (HAC) standard errors in all the inferential tests. Following a HAC correction, cumulative UV is the strongest predictor. The rate of tensile strength degradation with respect to cumulative UV exposure was estimated at 0.21 - 0.22 MPa per MJ/m2, based on ordinary least squares (OLS), multiple regression, and weighted least squares (WLS) models applied following the Breusch-Pagan test for heteroscedasticity. The second-order regression model gave a better predictive performance with R2 = 0.9686 and RMSE = 3.033 MPa; six of the nine higher-order terms were found significant after HAC correction, whereas the UV Temperature interaction became insignificant, which demonstrates the practical effect of the autocorrelation correction. Weibull distribution fitting was the best performer, with shape parameter β = 15.87 and B10 tensile strength threshold of 193.14 MPa at approximately 15.4 years of field exposure. Cost benefit analysis showed that premium fluoropolymer backsheets had a net present value benefit of about $7.55 per module in comparison to 25-year design life. These results provide a model of PV backsheet degradation, which can be easily reproduced, and which can be directly applied to reliability-based design and cost-effective lifecycle models.